Thermal Properties Metric English Comments
Working Point 1130 °C
2070 °F
Viscosity 10<sup>4</sup> dPa s; ISO 7884-2
Schott Glass 8242 Borosilicate Glass
Borosilicate glass for sealing to Kovar metal and molybdenum, electrically highly insulating, low refractive index Clad tube for optical fibers, glass metal sealing The heavy metal content for the..
Working Point 1130 °C
2070 °F
Viscosity 10<sup>4</sup> dPa s; ISO 7884-2
Schott Glass 8688 Borosilicate Glass
Borosilicate glass, highly UV-blocked, stabilized against solarization, sealing glass to Tungsten Backlights The heavy metal content of the elements lead, cadmium, mercury, and hexavalent chromium..