Thermal Properties | Metric | English | Comments |
---|---|---|---|
Working Point | 1068 °C | 1954 °F | 10<sup>4</sup> Poise |
Corning 7070 Lithia Potash Borosilicate Crushed/Powdered Glass Available in mesh sizes 4 through 325 and can be customized. Devitrifies before reaching a softening point. Used for sealing and other applications.Information provided by Corning Incorporated. |