Thermal Properties Metric English Comments
UL RTI, Mechanical with Impact 70.0 °C

@Thickness >=2.10 mm
158 °F

@Thickness >=0.0827 in
LG Chemical AF312B ABS, Flame Retardant
Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical..
UL RTI, Mechanical with Impact 70.0 °C

@Thickness >=2.50 mm
158 °F

@Thickness >=0.0984 in
LG Chemical AF312B ABS, Flame Retardant
Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical..
UL RTI, Mechanical with Impact 70.0 °C

@Thickness >=3.00 mm
158 °F

@Thickness >=0.118 in
LG Chemical AF312B ABS, Flame Retardant
Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical..