Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical with Impact | 150 °C @Thickness 0.810 mm |
302 °F @Thickness 0.0319 in |
(ALL) |
Hexion Bakelite™ PF 2736 Phenolic Formaldehyde Resin, Improved Electrical Properties, Low Shrinkage, UL Listed
&nbs Phenolic molding compound, inorganically/organically filled, increased tracking resistance, UL listed molding compound 0.46 mm/V-0 (BK, Suffix "H"), 0.81 mm/V-0 (NC, GN, BK), 1.5 mm/V-0 (ALL).Applic.. |
|||
UL RTI, Mechanical with Impact | 150 °C @Thickness 0.460 mm |
302 °F @Thickness 0.0181 in |
(BK suffix H) |
Hexion Bakelite™ PF 2736 Phenolic Formaldehyde Resin, Improved Electrical Properties, Low Shrinkage, UL Listed
&nbs Phenolic molding compound, inorganically/organically filled, increased tracking resistance, UL listed molding compound 0.46 mm/V-0 (BK, Suffix "H"), 0.81 mm/V-0 (NC, GN, BK), 1.5 mm/V-0 (ALL).Applic.. |
|||
UL RTI, Mechanical with Impact | 150 °C @Thickness 3.00 mm |
302 °F @Thickness 0.118 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® HTN 51G45HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN51G45HSL BK083 is a 45% glass reinforced, heat stabilized, lubricated high performance polyamide resin. It is also a PPA resin.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical with Impact | 150 °C @Thickness 0.750 mm |
302 °F @Thickness 0.0295 in |
UL746B |
DSM Arnite® TV4 260 SF PBT-30% Glass Reinforced (European and Asian Grade)
(discontinued **) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
UL RTI, Mechanical with Impact | 150 °C @Thickness 1.50 mm |
302 °F @Thickness 0.0591 in |
UL746B |
DSM Arnite® TV4 260 SF PBT-30% Glass Reinforced (European and Asian Grade)
(discontinued **) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |