Thermal Properties Metric English Comments
Glow Wire Test 849 °C

@Thickness 2.00 mm
1560 °F

@Thickness 0.0787 in
IEC 60695-2-13
Styron CALIBREâ„¢ 200-14 Polycarbonate Resin
Overview: CALIBREâ„¢ 200-14 polycarbonate resin is a natural, FDA compliant, 14 melt flow rate general purpose polycarbonate resin with no mold release or UV stabilizer.Govt. and Industry Standar..