Polymer Property : Glow Wire Test = 1650 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glow Wire Test 900 °C
1650 °F
IEC 60695-2-13
SABIC Innovative Plastics Lexan® FXD173R PC (Europe-Africa-Middle East)
LEXAN FXD173R is a UV stabilized translucent high flow grade for light diffusion special effects. The color package may affect performance.
Glow Wire Test 900 °C
1650 °F
IEC 60695-2-13
SABIC Innovative Plastics Lexan® EXL9330S PC Copolymer
Opaque PC-Siloxane copolymer with excellent processability. UV stabilized. UL rated V-0/5VA/CTI-PLC-2. Available in limited colors.
Glow Wire Test 900 °C
1650 °F
IEC 60695-2-13
SABIC Innovative Plastics Lexan® EXL9330S PC Copolymer (Asia Pacific)
Opaque PC-Siloxane copolymer with excellent processability. UV stabilized. UL rated V-0/5VA/CTI-PLC-2. Available in limited colors.
Glow Wire Test 900 °C
1650 °F
IEC 60695-2-13
SABIC Innovative Plastics Lexan® EXL9330S PC Copolymer (Europe-Africa-Middle East)
Opaque PC-Siloxane copolymer with excellent processability. UV stabilized. UL rated V-0/5VA/CTI-PLC-2. Available in limited colors.
Glow Wire Test 900 °C
1650 °F
GWIT at 1.0 mm; IEC 60695-2-13
Lavergne VYPET VNT 615 FR PET 15% Glass Reinforced, Flame Retardant
Vypet VNT 615 FR is a 15% fiberglass reinforced flame retardant PET injection molding compound designed for electrical and structural applications.Features: Flame retardant; UL yellow card file E216..