Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glow Wire Test | 650 - 750 °C | 1200 - 1380 °F | Average value: 730 °C Grade Count:5 |
Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45.. |
|||
Glow Wire Test | 650 - 750 °C | 1200 - 1380 °F | Average value: 664 °C Grade Count:6 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded". Each property range of values reported i.. |
|||
Glow Wire Test | 550 - 750 °C | 1020 - 1380 °F | Average value: 728 °C Grade Count:32 |
Overview of materials for Polypropylene with 30% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Talc Filler". Specific grades with primary filler content between 25% and 34% are.. |
|||
Glow Wire Test | 650 - 750 °C | 1200 - 1380 °F | Average value: 683 °C Grade Count:3 |
Overview of materials for Polypropylene with 10% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Talc Filler". Specific grades with primary filler content between 5% and 14% are .. |
|||
Glow Wire Test | 650 - 750 °C | 1200 - 1380 °F | Average value: 742 °C Grade Count:47 |
Overview of materials for Polypropylene with 40% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Talc Filler". Specific grades with primary filler content between 35% and 44% are.. |
|||
Glow Wire Test | 650 - 750 °C | 1200 - 1380 °F | Average value: 683 °C Grade Count:3 |
Overview of materials for Polypropylene, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum .. |