Thermal Properties | Metric | English | Comments |
---|---|---|---|
Strain Point | 521 °C | 970 °F | |
Corning Borosilicate Specialty Glass Pressed Parts Used as commercial residential lighting components (PAR) for halogen display lighting. Pressed borosilicate lenses and reflectors are highly durable and heat resistant making them ideally suited fo.. |