Thermal Properties | Metric | English | Comments |
---|---|---|---|
Strain Point | 440 °C | 824 °F | |
Corning 7052 Alkali Barium Borosilicate Crushed/Powdered Glass Available in mesh sizes 4 through 325 and can be customized. Used for sealing and other applications.Information provided by Corning Incorporated. |