Thermal Properties | Metric | English | Comments |
---|---|---|---|
Strain Point | 1106 °C | 2023 °F | |
Momentive Performance Materials Type 219 Fused Quartz Tubing Known as "Ozone-Free" or "Germicidal" quartz tubing. Transmits UV-A and UV-B while blocking the deep, high energy wavelengths that cause ozone generation and pose the greatest exposure risks. Tran.. |