Thermal Properties | Metric | English | Comments |
---|---|---|---|
Sublimation Temperature | 440 °C | 824 °F | |
Chengdu Polyster MCA Melamine Cyanurate White crystal power with satiny. It is an excellent non-halogen N flame retardant. The product is mainly used as non-halogen flame retardant for synthetic resin(PA, PVC, PS, POM), synthetic rubber a.. |