Thermal Properties | Metric | English | Comments |
---|---|---|---|
Sublimation Temperature | 2300 - 2500 °C | 4170 - 4530 °F | |
Specialty Materials SCS-6 Silicon Carbide Monofilament High strength at high temperature. These fibers are used in metal, ceramic and polymer matrix composites and are extremely effective for high-temperature applications. Silicon carbide reinforced tit.. |