Thermal Properties Metric English Comments
Pour Point 20.0 °C
68.0 °F
Solvay ANTAROX® PL 122 Surfactant
Description: General purpose dispersing agent.Chemical Name: ETHYLENE/PROPYLENE OXIDE BLOCK POLYMERCAS: 9003 – 11 – 6Solubility Dispersible in water. Soluble in most polar and aromatic sol..
Pour Point 20.0 °C
68.0 °F
Solvay RHODASURF® 870 Surfactant
Identification: ETHOXYLATED FATTY ALCOHOLCAS: 24938 – 91 – 8Available in: Asia Pacific, Europe, Latin America and North AmericaSolubility: Soluble in water and most polar and aromatic solvents. Ap..