Thermal Properties Metric English Comments
Pour Point -1.00 °C
30.2 °F
ExxonMobil Vacmul 3 A
Vacmul 3 A is a non-staining, low-viscosity mineral oil, intended for use as an EDM fluid or as a light- to moderate-duty honing oil.
Pour Point -1.00 °C
30.2 °F
ExxonMobil Vacmul 3 A
Vacmul 3 A is a non-staining, low-viscosity mineral oil, intended for use as an EDM fluid or as a light- to moderate-duty honing oil.