Thermal Properties | Metric | English | Comments |
---|---|---|---|
Pour Point | -4.00 °C | 24.8 °F | |
ChevronTexaco Pinnacle® 680 Texaco Pinnacle oils deliver value through:Long lubricant life in high temperature operations — The synthetic hydrocarbon base oils and proprietary additive package used in these products provide o.. |
|||
Pour Point | -4.00 °C | 24.8 °F | |
ChevronTexaco Pinnacle® 460 Texaco Pinnacle oils deliver value through:Long lubricant life in high temperature operations — The synthetic hydrocarbon base oils and proprietary additive package used in these products provide o.. |
|||
Pour Point | -4.00 °C | 24.8 °F | ASTM D97 |
ChevronTexaco Bright-Cut® AM Metal Working Fluid FeaturesChevron Bright-Cut Metalworking Fluids are a complete line of chlorine-free cutting oils that offer benefits not found in conventional cutting oils.The unique synthetic antiweld components .. |