Thermal Properties | Metric | English | Comments |
---|---|---|---|
Pour Point | 16.0 °C | 60.8 °F | |
Solvay ALKAMULS® OR 40 Surfactant Description: Biodegradable castor oil ethoxylate emulsifier, solubiliser for a wide range of formulations with an HLB of around 14.Identification: ETHOXYLATED CASTOR OILCAS: 61791 – 12 – 6.. |
|||
Pour Point | 16.0 °C | 60.8 °F | |
Solvay GERONOL® FF/6 Surfactant Description: Multipurpose emulsifier for EC, to use in pair with Geronol FF/4 or Rhodacal 70/B.Identification: BLENDED EMULSIFIERSSolubility: Soluble in water and most polar and aromatic solventsAva.. |