Thermal Properties | Metric | English | Comments |
---|---|---|---|
Pour Point | 15.0 °C | 59.0 °F | |
Solvay ALKAMULS® S 20 Surfactant Identification: SORBITAN MONOLAURATECAS: 1338 – 39 – 2EINECS : 215 – 663 – 3Solubility: Dispersible in water. Soluble in most polar and aromatic solvents.Available in: Asia Pacif.. |
|||
Pour Point | 15.0 °C | 59.0 °F | |
Solvay ANTAROX® B/848 Surfactant Description: Butyl EO.PO block polymer. Multipurpose emulsifier. Dispersing agent. Suggested for emulsifiable concentrates with polar solvents.Identification: ETHOPROPOXYLATED ALCOHOLCAS: 221045 â€.. |
|||
Pour Point | 15.0 °C | 59.0 °F | |
Solvay GERONOL® FF/6-E Surfactant Description: Multipurpose emulsifier for EC, to use in pair with Geronol FF/4 or Rhodacal 70/B.Identification: BLENDED EMULSIFIERSSolubility: Dispersible in water. Soluble in most polar and aromatic.. |
|||
Pour Point | 15.0 °C | 59.0 °F | |
Solvay GERONOL® MS Surfactant Description: Multipurpose emulsifier for EC, to use in pair with Geronol FF/4 or Rhodacal 70/B.Identification: BLENDED EMULSIFIERSSolubility: Soluble in water and most polar and aromatic solventsAva.. |
|||
Pour Point | 15.0 °C | 59.0 °F | |
Solvay GERONOL® TE 300 Surfactant Description: Emulsifier for agrochemical formulations.Identification: BLENDED EMULSIFIERSSolubility: Dispersible in water. Soluble in most polar and aromatic solventsAvailable in: Asia Pacific, Euro.. |
|||
Pour Point | 15.0 °C | 59.0 °F | |
Solvay LUBRHOPHOS® LB 400 E Surfactant Identification: ETHOXYLATED OELYL-CETYL ALCOHOL, PHOSPHATE ESTERSolubility: Dispersible in water. Soluble in most polar and aromatic solvents.Available in: Asia Pacific, Europe, Latin America and No.. |
|||
Pour Point | 15.0 °C | 59.0 °F | |
Solvay SOPROPHOR® 4 D 384 Surfactant Description: Multipurpose dispersing agent for SC formulationsIdentification: POLYARYLPHENYL ETHER SULPHATE, AMMONIUM SALTSolubility: Soluble in water and most polar and aromatic solvents.Available .. |
|||
Pour Point | 15.0 °C | 59.0 °F | |
Solvay SOPROPHOR® BSU Surfactant Description: Multipurpose dispersing agent for SC formulationsIdentification: ETHOXYLATED TRISTYRYLPHENOLCAS: 99734 – 09 – 5Solubility: Soluble in water and most polar and aromatic solvent.. |
|||
Pour Point | 15.0 °C | 59.0 °F | ASTM D97 |
ExxonMobil 26M Mobilgear SHC Mobilgear SHC 22M and 46M are supreme performance ultra high viscosity synthetic lubricants designed specifically for use in heavily loaded, low speed gears where boundary lubrication conditions oft.. |
|||
Pour Point | 15.0 °C | 59.0 °F | ASTM D97 |
ExxonMobil 26M Mobilgear SHC Mobilgear SHC 22M and 46M are supreme performance ultra high viscosity synthetic lubricants designed specifically for use in heavily loaded, low speed gears where boundary lubrication conditions oft.. |