Thermal Properties | Metric | English | Comments |
---|---|---|---|
Pour Point | -78.0 °C | -108 °F | |
PolyOne Synplast™ DOZ-E Di (2-ethylhexyl) Azelate Branched C8 azelate ester with antioxidantContains 0.10-0.15 wt% 1,1,3-Tris (2-methyl-4hydroxy-5-t-butyl phenyl) butane antioxidantInformation provided by PolyOne |
|||
Pour Point | -78.0 °C | -108 °F | |
3M Novec™ 774 Engineered Fluid 3M™ Novec™ 774 Engineered Fluid is a clear, colorless and low odor fluid, and is one in a line of 3M products designed as replacements for ozone depleting substances (ODSs) and compounds with high.. |