Polymer Property : Pour Point = -71.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Pour Point -71.0 °C
-95.8 °F
Base Oil; ASTM D97
Nye Lubricants UniFlor 8730 (UF) Synthetic Oil
Information provided by Nye Lubricants.
Pour Point -71.0 °C
-95.8 °F
Base Oil; ASTM D97
Nye Lubricants UniFlor 8731 (UF) Synthetic Oil
Information provided by Nye Lubricants.