Polymer Property : Pour Point = -47.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Pour Point -47.0 °C
-52.6 °F
Base Oil; ASTM D97
Nye Lubricants 590 (SO) Synthetic Oil
Information provided by Nye Lubricants.
Pour Point -47.0 °C
-52.6 °F
PolyOne Synplast™ DOP-N Di (2-ethylhexyl) Phthalate
Branched C8 phthalate esterInformation provided by PolyOne
Pour Point -47.0 °C
-52.6 °F
Base Oil; ASTM D97
Nye Lubricants 345 (SO) Synthetic Oil
Information provided by Nye Lubricants.
Pour Point -47.0 °C
-52.6 °F
ChevronTexaco Inhibited Transformer Oil
Texaco Transformer Oil and Texaco Transformer Oil Inhibited deliver value through:Prolonged transformer life — Excellent conductive heat transfer properties improve cooling of transformer component..
Pour Point -47.0 °C
-52.6 °F
ChevronTexaco Transformer Oil
Texaco Transformer Oil and Texaco Transformer Oil Inhibited deliver value through:Prolonged transformer life — Excellent conductive heat transfer properties improve cooling of transformer component..
Pour Point -47.0 °C
-52.6 °F
ASTM D97
ChevronTexaco Cetus® PAO 100
Texaco Cetus PAO oils deliver value through:Long lubricant life in high temperature operations — Outstanding thermal and oxidation stability.Extended machinery life and increased compressor efficie..
Pour Point -47.0 °C
-52.6 °F
ASTM D97
ChevronTexaco Clarity® 10W-20 Synthetic Hydraulic Oil AW
Chevron Clarity Synthetic Hydraulic Oil AW is designed to give maximum protection to both mobile and stationary hydraulic pumps in high-performance industrial applications as well as in environmenta..