Thermal Properties | Metric | English | Comments |
---|---|---|---|
Pour Point | -31.0 °C | -23.8 °F | Base Oil; ASTM D97 |
Nye Lubricants 863 (FG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -31.0 °C | -23.8 °F | ASTM D97 |
ChevronTexaco Delo® 400 SAE 30 Chevron Delo 400 heavy duty motor oils are exceptional, super premium quality “universal” engine oils which exceed industry and engine manufacturers’ performance requirements.They are formulated .. |
|||
Pour Point | -31.0 °C | -23.8 °F | ASTM D97 |
ChevronTexaco Delo® 400 SAE 50 Chevron Delo 400 heavy duty motor oils are exceptional, super premium quality “universal” engine oils which exceed industry and engine manufacturers’ performance requirements.They are formulated .. |
|||
Pour Point | -31.0 °C | -23.8 °F | |
ChevronTexaco Pinnacle® 220 Texaco Pinnacle oils deliver value through:Long lubricant life in high temperature operations — The synthetic hydrocarbon base oils and proprietary additive package used in these products provide o.. |
|||
Pour Point | -31.0 °C | -23.8 °F | |
ChevronTexaco URSA® SAE 30 Premium TDX Texaco Ursa Premium TDX delivers value through:Reduced wear — Prolonging component life and providing reduced maintenance costs.Improved engine cleanliness — Providing efficient operation and redu.. |
|||
Pour Point | -31.0 °C | -23.8 °F | |
ChevronTexaco Pinnacle® 320 Texaco Pinnacle oils deliver value through:Long lubricant life in high temperature operations — The synthetic hydrocarbon base oils and proprietary additive package used in these products provide o.. |