Thermal Properties | Metric | English | Comments |
---|---|---|---|
Pour Point | -33.9 °C | -29.0 °F | |
ConocoPhillips Hydroclear® 30 Power-D E.O. 30 Description: Conoco Hydroclear Power-D Engine Oil, formulated from Conoco's premium hydrocracked base stock, protects diesel and gasoline engines against wear, deposits, varnish, rust and corros.. |
|||
Pour Point | -33.9 °C | -29.0 °F | |
ConocoPhillips Hydroclear® El Mar® 15W-40 Ashless Heavy Duty Description: Conoco Hydroclear El Mar Ashless Heavy Duty is a high-quality, ashless natural gas engine oil formulated from exclusive Conoco hydrocracked base stock. Hydroclear El Mar Ashless Heavy D.. |
|||
Pour Point | -33.9 °C | -29.0 °F | |
ConocoPhillips Hydroclear® El Mar® Ashless Heavy Duty SAE 40 Description: Conoco Hydroclear El Mar Ashless Heavy Duty is a high-quality, ashless natural gas engine oil formulated from exclusive Conoco hydrocracked base stock. Hydroclear El Mar Ashless Heavy D.. |