Thermal Properties Metric English Comments
Pour Point <= -115 °C
<= -175 °F
Solvay Specialty Polymers Galden® HT55 PFPE Heat Transfer Fluid
Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service..