Thermal Properties | Metric | English | Comments |
---|---|---|---|
Pour Point | -18.3 °C | -1.00 °F | |
Duratherm 630 Paraffinic Heat Transfer Fluid Duratherm 630 - rated to 630°F it has the highest rated bulk temperature of petroleum based thermal fluids. Duratherm 630 is engineered for applications requiring high temperature stability (630°F.. |