Polymer Property : UL RTI, Mechanical without Impact = 220 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
UL RTI, Mechanical without Impact 150 - 220 °C
302 - 428 °F
Average value: 203 °C Grade Count:127
Overview of materials for Silicone, Molded, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Silicone, Molded, Glass Fiber Filled". Each property range of values reported is minimum and maximum val..
UL RTI, Mechanical without Impact 65.6 - 220 °C
150 - 428 °F
Average value: 202 °C Grade Count:135
Overview of materials for Silicone Rubber
This property data is a summary of similar materials in the MatWeb database for the category "Silicone Rubber". Each property range of values reported is minimum and maximum values of appropriate Ma..