Polymer Property : UL RTI, Mechanical with Impact = 185 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
UL RTI, Mechanical with Impact 50.0 - 85.0 °C
122 - 185 °F
Average value: 62.0 °C Grade Count:20
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded". Each property range of values reported i..
UL RTI, Mechanical with Impact 10.0 - 85.0 °C
50.0 - 185 °F
Average value: 59.7 °C Grade Count:35
Overview of materials for PVC, Rigid Grade
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Rigid Grade". Each property range of values reported is minimum and maximum values of appropriate M..