Polymer Property : UL RTI, Mechanical with Impact = 125 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
UL RTI, Mechanical with Impact 125 °C
257 °F
UL 746B
SABIC Innovative Plastics Lexan® 101R PC (Europe-Africa-Middle East)
LEXAN 101R is a high viscosity multi purpose grade and contains a release agent to ensure easy processing. LEXAN 101R is available in transparent, translucent and opaque colours.
UL RTI, Mechanical with Impact 125 °C
257 °F
UL 746B
SABIC Innovative Plastics Lexan® 103R PC (Europe-Africa-Middle East)
LEXAN 103R is a high viscosity multi purpose U.V. stabilized grade and contains a release agent to ensure easy processing. LEXAN 103R is available in transparent, translucent and opaque colours.
UL RTI, Mechanical with Impact 125 °C
257 °F
UL 746B
SABIC Innovative Plastics Lexan® 141 PC (Europe-Africa-Middle East)
LEXAN 141 is a medium viscosity multi purpose grade available in transparent, translucent and opaque colours.
UL RTI, Mechanical with Impact 125 °C
257 °F
UL 746B
SABIC Innovative Plastics Lexan® 161 PC (Europe-Africa-Middle East)
LEXAN 161 is a medium viscosity multi purpose grade available in transparent, translucent and opaque colours.
UL RTI, Mechanical with Impact 125 °C
257 °F
UL 746B
SABIC Innovative Plastics Lexan® 161R PC (Europe-Africa-Middle East)
LEXAN 161R is a medium viscosity multi purpose grade and contains a release agent to ensure easy processing. LEXAN 161R is available in transparent, translucent and opaque colours.
UL RTI, Mechanical with Impact 125 °C
257 °F
UL 746B
SABIC Innovative Plastics Lexan® 201R PC (Europe-Africa-Middle East)
LEXAN 201R is a high viscosity multi purpose grade and contains a release agent to ensure easy processing. This grade is UL94-V2 at 0.8 mm approved.
UL RTI, Mechanical with Impact 125 °C
257 °F
UL 746B
SABIC Innovative Plastics Lexan® 241 PC (Europe-Africa-Middle East)
LEXAN 241 resin is a medium viscosity multi purpose polycarbonate with UL94-V2 rated. All color options are available.
UL RTI, Mechanical with Impact 125 °C
257 °F
UL 746B
SABIC Innovative Plastics Lexan® 243R PC (Europe-Africa-Middle East)
LEXAN 243R is a medium viscosity multi purpose UV stabilized grade and contains release agent to ensure easy processing. This grade is UL94-V2 at 0.8 mm approved.
UL RTI, Mechanical with Impact 125 °C
257 °F
UL 746B
SABIC Innovative Plastics Lexan® 4501 PPC (Asia Pacific)
High heat resistant polyphthlate carbonate, provides DTUL of 290F at 264 psi.
UL RTI, Mechanical with Impact 125 °C
257 °F
UL 746B
SABIC Innovative Plastics Lexan® 4504 PPC
High heat resistant polycarbonate copolymer, provides DTUL of 290F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported with ..
UL RTI, Mechanical with Impact 125 °C
257 °F
UL 746B
SABIC Innovative Plastics Lexan® 4504 PPC (Asia Pacific)
High heat resistant polycarbonate copolymer, provides DTUL of 290F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported wit..
UL RTI, Mechanical with Impact 125 °C
257 °F
UL 746B
SABIC Innovative Plastics Lexan® FXE101R PC (Europe-Africa-Middle East)
Transparent PC. ILLUMINATE special effects (fluorescent/edge glow colors). For thicker sections without sinks. Internal mold release.This data was supplied by SABIC-IP for the Europe-Africa-Middl..
UL RTI, Mechanical with Impact 125 °C
257 °F
UL 746B
SABIC Innovative Plastics Lexan® GLX143 PC (Europe-Africa-Middle East)
Lexan* GLX resin is a medium viscosity grade which is an excellent candidate for applications with high optical quality requirements, such as automotive glazing applications. Available in transparen..
UL RTI, Mechanical with Impact 125 °C
257 °F
UL 746B
SABIC Innovative Plastics Lexan® HP2REU PC (Europe-Africa-Middle East)
Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains a h..
UL RTI, Mechanical with Impact 125 °C
257 °F
UL 746B
SABIC Innovative Plastics Lexan® HPH4504 PPC (Asia Pacific)
High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, steam, gamma and e-beam steril..
UL RTI, Mechanical with Impact 125 °C
257 °F
UL 746B
SABIC Innovative Plastics Lexan® HPH4504 PPC (Europe-Africa-Middle East)
High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, steam, gamma and e-beam steril..
UL RTI, Mechanical with Impact 125 °C
257 °F
UL 746B
SABIC Innovative Plastics Lexan® LS1 PC (Europe-Africa-Middle East)
LEXAN LS1 is a low viscosity injection moulding grade especially designed for manufacturing complex parts requiring easy flow properties combined with high optical requirements.
UL RTI, Mechanical with Impact 125 °C
257 °F
UL 746B
SABIC Innovative Plastics Lexan® LUX2010T_ PC (Europe-Africa-Middle East)
Global grade. LEXAN LUX2010T is an injection moulding grade especially designed for manufacturing optical parts requiring excellent flow properties combined with very high transmission and color sta..
UL RTI, Mechanical with Impact 125 °C
257 °F
UL 746B
SABIC Innovative Plastics Lexan® LUX2110T_ PC (Europe-Africa-Middle East)
Global grade. LEXAN LUX2110T is an injection moulding grade especially designed for manufacturing optical parts requiring easy flow properties combined with very high transmission and color stabilit..
UL RTI, Mechanical with Impact 125 °C
257 °F
UL 746B
SABIC Innovative Plastics Lexan® LUX2180T_ PC (Europe-Africa-Middle East)
Global grade. LEXAN LUX2180T is an injection moulding grade especially designed for manufacturing optical parts requiring easy flow properties combined with very high transmission and color stabilit..
UL RTI, Mechanical with Impact 125 °C
257 °F
UL 746B
SABIC Innovative Plastics Lexan® LUX2910 PC (Asia Pacific)
Global grade. LEXAN LUX2910 is an injection moulding grade especially designed for manufacturing optical parts requiring superior flow properties combined with very high transmission and color stabi..
UL RTI, Mechanical with Impact 125 °C
257 °F
UL 746B
SABIC Innovative Plastics Lexan® ML104R PC (Europe-Africa-Middle East)
LEXAN ML104R is a high viscosity multi purpose grade. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade will no longer be supported with biocompatibility inform..
UL RTI, Mechanical with Impact 125 °C
257 °F
UL 746B
SABIC Innovative Plastics Lexan® OQ3420 PC (Europe-Africa-Middle East)
Medium Viscosity, UV-stabilized grade for ophthalmic lenses.
UL RTI, Mechanical with Impact 125 °C
257 °F
UL 746B
SABIC Innovative Plastics Lexan® 221R PC (Europe-Africa-Middle East)
LEXAN 221R is a low viscosity multi purpose grade and contains a release agent to ensure easy processing. This grade is UL94-V2 at 0.4 mm approved.
UL RTI, Mechanical with Impact 125 °C
257 °F
UL 746B
SABIC Innovative Plastics Lexan® ML3999 PC (Europe-Africa-Middle East)
LEXAN ML3999 is a medium viscosity, 20% glass reinforced grade. It offers excellent flame retardancy and is especially designed for applications requiring high rigidity together with high heat.
UL RTI, Mechanical with Impact 125 °C
257 °F
UL 746B
SABIC Innovative Plastics LNP Thermocomp RF00ASXP PA6.6 (Europe-Africa-Middle East)
LNP* THERMOCOMP* RF00ASXP is a compound based on PA 66 resin containing Glass Fiber. Added features include: Heat Stabilized.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regi..
UL RTI, Mechanical with Impact 125 °C
257 °F
UL 746B
SABIC Innovative Plastics LNP THERMOCOMP WF0049 PBT (Europe-Africa-Middle East)
LNP* Thermocomp* WF0049 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant.
UL RTI, Mechanical with Impact 125 °C
257 °F
UL 746B
SABIC Innovative Plastics NORYL LTA6020 PPE+PS (Europe-Africa-Middle East)
UL RTI, Mechanical with Impact 125 °C
257 °F
Eurostar Staramide RF00ASXP PA66, 50% Glass Filled, Injection Molded
Staramide RF00ASXP is a 50% Glass Fiber Reinforced Polyamide 66 Injection Molding Resin (also known as Staramide 66 G 50V S3)Information provided by Eurostar.
UL RTI, Mechanical with Impact 125 °C
257 °F
UL 746B
SABIC Innovative Plastics Lexan® HPH4504H PPC
High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, ..