Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Electrical | 230 °C | 446 °F | 0.0625 in; UL 746 |
LyondellBasell Hostacom™ PF062-3 Polypropylene Homopolymer Description: Hostacom™ PF062-3 high melt flow, 5,200 MPa flexural modulus, chemically coupled, 30% glass fiber-reinforced polypropylene homopolymer has good impact strength, high stiffness and very.. |