Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 96.7 °C
206 °F
ASTM D648
RheTech Products FT7013-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Scuff platesLift gate coversI/P componentsClose-out panelsInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 0.46 MPa (66 psi) 96.7 °C
206 °F
ASTM D648
RheTech Products FT7013-720UV Thermoplastic Polyolefin, UV Stabilized, XTM Dark Sandstone
Applications: Scuff platesLift gate coversI/P componentsClose-out panelsInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 0.46 MPa (66 psi) 96.7 °C
206 °F
ASTM D648
RheTech Products FT7013-721UV Thermoplastic Polyolefin, UV Stabilized, XDV Dark Slate
Applications: Scuff platesLift gate coversI/P componentsClose-out panelsInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 0.46 MPa (66 psi) 96.7 °C
206 °F
Unannealed; ASTM Data
Americas Styrenics Styron® 685 Polystyrene  (discontinued **)
STYRON® 685 general purpose polystyrene resin is a high heat resin used in consumer electronics and housewares. It offers excellent clarity, good moldability for use in hot runner systems. When use..
Deflection Temperature at 0.46 MPa (66 psi) 96.7 °C
206 °F
Unannealed; ASTM Data
Americas Styrenics Styron® 685P Polystyrene  (discontinued **)
STYRON® 685P general purpose polystyrene resin is a high heat resin with good strength, moldability/processability, and excellent clarity. This resin is typically used in consumer electronic applic..
Deflection Temperature at 0.46 MPa (66 psi) 96.7 °C
206 °F
Unannealed; ASTM D648
Styron MAGNUMâ„¢ 3325 SLG Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: Super Low Gloss, Medium Heat, Medium Impact ABS resin for injection molded automotive interior trim applications Magnum 3325 SLG can achieve 60° Gardner gloss levels below 2.0 with low ..
Deflection Temperature at 0.46 MPa (66 psi) 96.7 °C
206 °F
ASTM D648
ExxonMobil PP7654KNE2 Polypropylene Homopolymer
Product Description: A high impact copolymer resin with medium melt flow rate and excellent processing attributes. It is designed for injection molded large consumer and industrial parts.Availabili..
Deflection Temperature at 0.46 MPa (66 psi) 96.7 °C
206 °F
Unannealed; ASTM D648
Entec Hyril® GP355AS Styrene Acrylonitrile
Available in North America Features: Copolymer Automotive Specifications: DELPHI M-9565-9 Color: Blue-TransparentForm: PelletsProcessing Method: ExtrusionInformation provided by Entec
Deflection Temperature at 0.46 MPa (66 psi) 96.7 °C
206 °F
Unannealed; ASTM D648
Entec Hyril® SAN500 Styrene Acrylonitrile
Available in North America Features: Copolymer Form: PelletsInformation provided by Entec
Deflection Temperature at 0.46 MPa (66 psi) 96.7 °C
206 °F
ASTM D648
Americas Styrenics STYRON® 610 High Heat Crystal Polystyrene
Product CharacteristicsAdditive freeTypical ApplicationsFoamsFilms/opticalCarrier resinSpecialty blendingInformation provided by AmericasStyrenics LLC.