Deflection Temperature at 0.46 MPa (66 psi) 85.0 - 87.0 °C
185 - 189 °F
C.O.I.M. EXTER S® S 702 Self-extinguishing Resin
Description: The Exter S product line contains a large number of unsaturated polyester resin products with an array of properties and applications.Specific Notes for ESTER S® S 702: High-performanc..