Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 72.00 °C
161.6 °F
ASTM D-648
Axiall CL-6380, CL-6380J Rigid PVC, Molding
Georgia Gulf CL-6380 & CL-6380J are clear fittings compounds with cell class 12454(Type 1, Grade 1). These compounds are ideally suited for swimming pools, spas, and numerous applications where vis..
Deflection Temperature at 0.46 MPa (66 psi) 72.00 °C
161.6 °F
ASTM D-648
Axiall HF-6597 Rigid PVC, Molding
Georgia Gulf HF-6597 is a high flow PVC compound designed for thin wall parts and multi-cavity molds. It is ideally suited for a variety of electrical and appliance applications.Information provide..
Deflection Temperature at 0.46 MPa (66 psi) 72.00 °C
161.6 °F
ASTM D-648
Axiall UV-6670 Rigid PVC, Molding
Georgia Gulf UV-6670 is a weatherable, high flow injection molding compound, specially formulated for outdoor UV exposure. This compound was designed to be used in various accessory parts, such as ..
Deflection Temperature at 0.46 MPa (66 psi) 72.00 °C
161.6 °F
ASTM D-648
Axiall UV-6676 Rigid PVC, Molding
Georgia Gulf UV-6676 is a weatherable, high flow injection molding compound, specially formulated for outdoor UV exposure. This compound was designed to be used in various accessory parts, such as ..
Deflection Temperature at 0.46 MPa (66 psi) 72.00 °C
161.6 °F
ASTM D-648
Axiall UV-6680 Rigid PVC, Molding
Georgia Gulf UV-6680 is a weatherable, high flow injection molding compound, specially formulated for outdoor UV exposure. This compound was designed to be used in various accessory parts, such as ..