Polymer Property : Deflection Temperature at 0.46 MPa (66 psi) = 69.4 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 69.4 °C
157 °F
ASTM D648
Ineos R08S-00 Polypropylene Random Copolymer
This is a medium flow rate random copolymer designed for extrusion processing requiring slip properties and meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177..