Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 58.0 - 68.0 °C
136 - 154 °F
ASTM D648-06
Proto3000 Objet Digital Materials™ RGD5160-DM ABS-like Prototyping Polymer
Objet ABS-like Digital Material made of Object RGD515 & Objet RGD535Digital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to..