Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 337 °C | 639 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP LUBRICOMP LFL36E PEEK LNP* LUBRICOMP* LFL36E is a compound based on Polyetheretherketone containing 30% Glass Fiber, 15% PTFE. Added features of this material are: Wear Resistant, Easy Molding. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 337 °C @Thickness 3.20 mm |
639 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP LF004E PEEK LNP* THERMOCOMP* LF004E is a compound based on Polyetheretherketone resin containing 20% Glass Fiber. Added features of this material include: Easy Molding. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 337 °C @Thickness 3.20 mm |
639 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP LX03447 PEEK LNP* THERMOCOMP* LX03447 is a compound based on Polyetheretherketone containing Proprietary Filler(s). |