Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 304 °C | 580 °F | Annealed, 0.125 in bars; ASTM D648 |
PolyOne Lubri-Tech™ AM-30CF/15T Polyphthalamide (PPA), Carbon Fiber Reinforced, PTFE Lubricated
(discontinued Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |