Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Deflection Temperature at 0.46 MPa (66 psi) = 56.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 56.0 °C
133 °F
120°C/h; ISO 75/1
Polykemi AB POLYelast TPE EC88R Thermoplastic Elastomer, PP/EPDM
Information provided by Polykemi AB
Deflection Temperature at 0.46 MPa (66 psi) 56.0 °C
133 °F
Reliance Industries Polypropylene - Virgin Polypropylene
Information provided by Reliance Industries
Deflection Temperature at 0.46 MPa (66 psi) 56.0 °C
133 °F
ASTM D648
Formosa Plastics Formolene® L43840U Rotational Molding LLDPE  (discontinued **)
Butene CopolymerApplications: Toys and other non-tank rotational molding applications.Formolene L43840U is a Butene Copolymer of linear low density polyethylene for toys and other non-tank rotationa..
Deflection Temperature at 0.46 MPa (66 psi) 56.0 °C
133 °F
ASTM D648
Formosa Plastics Formolene® L64220UT1 Rotational Molding LLDPE  (discontinued **)
Hexene CopolymerApplications: Large tanks, material handling equipment and industrial rotational molding applications.Formolene L64220U is fully heat and UV stabilized.Meets all requirements of the ..
Deflection Temperature at 0.46 MPa (66 psi) 56.0 °C
133 °F
ASTM D648
LyondellBasell Petrothene® GA694189 Linear Low Density Polyethylene, Injection Molding Grade
PETROTHENE GA694189 is a pelletized LLDPE copolymer resin for injection molding. Typical applications include lids and thin-walled items that require high flow and short cycle times. GA694189 exhibi..
Deflection Temperature at 0.46 MPa (66 psi) 56.0 °C
133 °F
ISO 75
GEHR Plastics ECOGEHR® PLA-LF Polylactic Acid
PLA-L is a blend of polylactide, lignin, lingo-cellulosic, natural fatty acids, waxes and wood fibers. This material possesses good mechanical properties similar to ABS. This bioplastic has an opera..
Deflection Temperature at 0.46 MPa (66 psi) 56.0 °C
133 °F
ASTM D648
LyondellBasell Astryn BB725GC Polypropylene Copolymer, Mineral Filled
Key Features: medium melt flow, medium high modulus, UV-stabilized, mineral-filled polypropylene copolymer, excellent impact and stiffness balance, good processability, good weatherability,Applicati..
Deflection Temperature at 0.46 MPa (66 psi) 56.0 °C
133 °F
ASTM D648
Samyang Triel® 5401BM Thermoplastics Polyetherester Elastomer, Blow Molding
Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5401BM is for blow molding applications.Applications: Automotive - CVJB and BellowsInformation provided ..
Deflection Temperature at 0.46 MPa (66 psi) 56.0 °C

@Thickness 3.20 mm
133 °F

@Thickness 0.126 in
ISO 75
A. Schulman FORMION™ FI 391 Ionomer
DescriptionFormion® FI 391 is a non-reinforced, injection molding grade Ionomer, which has been formulated for scratch resistance, low temperature ductility, and medium stiffness. Formion F1 391U i..
Deflection Temperature at 0.46 MPa (66 psi) 56.0 °C

@Thickness 3.20 mm
133 °F

@Thickness 0.126 in
ISO 75
A. Schulman FORMION™ FI 391 Ionomer
DescriptionFormion® FI 391 is a non-reinforced, injection molding grade Ionomer, which has been formulated for scratch resistance, low temperature ductility, and medium stiffness. Formion F1 391U i..
Deflection Temperature at 0.46 MPa (66 psi) 56.0 °C

@Thickness 3.20 mm
133 °F

@Thickness 0.126 in
ISO 75
A. Schulman FORMION™ FI 391 Ionomer
DescriptionFormion® FI 391 is a non-reinforced, injection molding grade Ionomer, which has been formulated for scratch resistance, low temperature ductility, and medium stiffness. Formion F1 391U i..
Deflection Temperature at 0.46 MPa (66 psi) 56.0 °C

@Thickness 3.20 mm
133 °F

@Thickness 0.126 in
ISO 75
A. Schulman FORMION™ FI 391 Ionomer
DescriptionFormion® FI 391 is a non-reinforced, injection molding grade Ionomer, which has been formulated for scratch resistance, low temperature ductility, and medium stiffness. Formion F1 391U i..
Deflection Temperature at 0.46 MPa (66 psi) 56.0 °C

@Thickness 3.20 mm
133 °F

@Thickness 0.126 in
ISO 75
A. Schulman FORMION™ FI 391 Ionomer
DescriptionFormion® FI 391 is a non-reinforced, injection molding grade Ionomer, which has been formulated for scratch resistance, low temperature ductility, and medium stiffness. Formion F1 391U i..
Deflection Temperature at 0.46 MPa (66 psi) 56.0 °C

@Thickness 3.20 mm
133 °F

@Thickness 0.126 in
ISO 75
A. Schulman FORMION™ FI 391 Ionomer
DescriptionFormion® FI 391 is a non-reinforced, injection molding grade Ionomer, which has been formulated for scratch resistance, low temperature ductility, and medium stiffness. Formion F1 391U i..
Deflection Temperature at 0.46 MPa (66 psi) 56.0 °C
133 °F
ASTM-D648
Braskem RA34U3 LLDPE Rotomolding Polyethylene
The resin RA34U3 is a linear low-density polyethylene, 1-butene based, with a good balance of processability, environmental stress cracking resistance, and impact strength. It contains long term UV6..
Copyright © lookpolymers.com All Rights Reserved