Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 215.4 °C | 419.7 °F | ISO 75-1,-2 |
Gromax BFG30-AH00B3 Nylon 6 30% Glass Filled (Conditioned) Information provided by Gromax Enterprises Corp. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 215.4 °C | 419.7 °F | ISO 75-1,-2 |
Gromax BFG30-AH00B3 Nylon 6 30% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |