Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 188 °C | 371 °F | ASTM D648 |
A. Schulman SCHULAMID® 66 MV3 Unreinforced Nylon 6/6 Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 188 °C | 371 °F | ASTM D648 |
A. Schulman SCHULAMID® 66 MV3H Unreinforced Nylon 6/6 Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 188 °C | 371 °F | ASTM D648 |
A. Schulman SCHULAMID® 66 MV3 Unreinforced Nylon 6/6 Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 188 °C | 371 °F | ASTM D648 |
A. Schulman SCHULAMID® 66 MV3H Unreinforced Nylon 6/6 Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 188 °C | 371 °F | ASTM D648 |
A. Schulman SCHULAMID® 66 MV3 Unreinforced Nylon 6/6 Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 188 °C | 371 °F | ASTM D648 |
A. Schulman SCHULAMID® 66 MV3H Unreinforced Nylon 6/6 Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 188 °C | 371 °F | ASTM D648 |
A. Schulman SCHULAMID® 66 MV3 Unreinforced Nylon 6/6 Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 188 °C | 371 °F | ASTM D648 |
A. Schulman SCHULAMID® 66 MV3H Unreinforced Nylon 6/6 Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 188 °C | 371 °F | ASTM D648 |
A. Schulman SCHULAMID® 66 MV3 Unreinforced Nylon 6/6 Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 188 °C | 371 °F | ASTM D648 |
A. Schulman SCHULAMID® 66 MV3H Unreinforced Nylon 6/6 Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 188 °C | 371 °F | ASTM D648 |
A. Schulman SCHULAMID® 66 MV3 Unreinforced Nylon 6/6 Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 188 °C | 371 °F | ASTM D648 |
A. Schulman SCHULAMID® 66 MV3H Unreinforced Nylon 6/6 Information provided by A. Schulman. |