Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 186 °C | 366 °F | Unannealed; ASTM D648 |
Techmer ES Luriblend® PA6/6 LX Nylon 66 Availability: North AmericaForms: PelletsFeatures: Good Wear Resistance and Low FrictionInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 186 °C | 366 °F | Unannealed; ASTM D648 |
Techmer ES Luriblend® PA6/6 X Nylon 66 Availability: North AmericaForms: PelletsAdditive: Lubricant Features: Lubricated, Good Wear Resistance and Low FrictionInformation provided by TP Composites, Inc. |