Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 341 °C @Thickness 3.20 mm |
646 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP LX08411 PEEK LNP* THERMOCOMP* LX08411 is a compound based on Polyetheretherketone resin containing Carbon Fiber. Added feature of this material is: Opaque. |