Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 160 - 171 °C
320 - 340 °F
Average value: 163 °C Grade Count:21
Overview of materials for Acetal Copolymer, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Carbon Fiber Filled". Each property range of values reported is minimum and maximum va..
Deflection Temperature at 0.46 MPa (66 psi) 73.9 - 171 °C
165 - 340 °F
Average value: 154 °C Grade Count:17
Overview of materials for Acetal Homopolymer, PTFE-Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, PTFE-Filled". Each property range of values reported is minimum and maximum values o..