Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 339 °C

@Thickness 3.20 mm
642 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP LUBRICOMP LFL36E PEEK
LNP* LUBRICOMP* LFL36E is a compound based on Polyetheretherketone containing 30% Glass Fiber, 15% PTFE. Added features of this material are: Wear Resistant, Easy Molding.