Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 133 - 169 °C
271 - 336 °F
Average value: 152 °C Grade Count:91
Overview of materials for Polypropylene, Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum ..