Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 33.9 °C | 93.0 °F | ASTM D648 |
Dow AMPLIFY™ VA 400 Ethylene vinyl acetate (EVA) AMPLIFY™ VA 400 Functional Polymer is produced via a high pressure reactor. It exhibits high flexibility, clarity and low temperature sealability. It is easy to process and features functional .. |