Deflection Temperature at 0.46 MPa (66 psi) 289 °C
552 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
SABIC Innovative Plastics LNP LUBRICOMP 9X98026 PA 46 (Europe-Africa-Middle East)
LNP* Lubricomp* 9X98026 is a compound based on PA4.6 resin containing Barium Sulfate, PTFE and Carbon Fiber
Deflection Temperature at 0.46 MPa (66 psi) 289 °C
552 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
SABIC Innovative Plastics LNP LUBRICOMP UX06425 PPA
LNP* LUBRICOMP* UX06425 is a compound based on Polyphthalamide (PPA) containing 10% Glass Fiber, 10% PTFE. Added features of this material include: Wear Resistant, Hot Water Moldable and Heat Stab..
Deflection Temperature at 0.46 MPa (66 psi) 289 °C

@Thickness 3.20 mm
552 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP THERMOCOMP UF00BAS PPA
LNP* THERMOCOMP* UF00BAS is a compound based on Polyphthalamide containing 55% Glass Fiber. Added feature of this material is: Heat Stabilized.