Deflection Temperature at 0.46 MPa (66 psi) 287 °C
549 °F
HDT B; Unannealed; ISO 75-2/B
Solvay Specialty Polymers Xydar® MG-850 Liquid Crystal Polymer (LCP), 50% GlassMineral
Xydar® MG-850 liquid crystal polymer (LCP) is a 50% glass/mineral reinforced injection molding grade developed for electrical/electronic applications utilizing surface mount technology. The mater..