Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 109 °C | 229 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 2181HU High Flow, Fortified, Impact Resistant Polypropylene DescriptionPolyfort® FPP 2181HU is a high flow, fortified, impact resistant polypropylene, stabilized for UV resistance, and available in automotive matched colors. Information provided by A. Schul.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 109 °C | 229 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 2181HU High Flow, Fortified, Impact Resistant Polypropylene DescriptionPolyfort® FPP 2181HU is a high flow, fortified, impact resistant polypropylene, stabilized for UV resistance, and available in automotive matched colors. Information provided by A. Schul.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 109 °C | 229 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 2181HU High Flow, Fortified, Impact Resistant Polypropylene DescriptionPolyfort® FPP 2181HU is a high flow, fortified, impact resistant polypropylene, stabilized for UV resistance, and available in automotive matched colors. Information provided by A. Schul.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 109 °C | 229 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 2181HU High Flow, Fortified, Impact Resistant Polypropylene DescriptionPolyfort® FPP 2181HU is a high flow, fortified, impact resistant polypropylene, stabilized for UV resistance, and available in automotive matched colors. Information provided by A. Schul.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 109 °C | 229 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 2181HU High Flow, Fortified, Impact Resistant Polypropylene DescriptionPolyfort® FPP 2181HU is a high flow, fortified, impact resistant polypropylene, stabilized for UV resistance, and available in automotive matched colors. Information provided by A. Schul.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 109 °C | 229 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 2181HU High Flow, Fortified, Impact Resistant Polypropylene DescriptionPolyfort® FPP 2181HU is a high flow, fortified, impact resistant polypropylene, stabilized for UV resistance, and available in automotive matched colors. Information provided by A. Schul.. |