Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 97.00 °C | 206.6 °F | ASTM D648 |
Noble Polymers Forte™ 4CPP093 Nanocomposite Forte is a polypropylene-based nanocomposite produced by Noble Polymers. It is one of the first commercialization of nanocomposites in the automotive industry and can be used in a variety of applica.. |