Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 77.0 - 96.0 °C | 171 - 205 °F | Average value: 84.8 °C Grade Count:53 |
Overview of materials for Cellulose Acetate Propionate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate Propionate, Molded". Each property range of values reported is minimum and maximum val.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 70.0 - 96.1 °C | 158 - 205 °F | Average value: 84.7 °C Grade Count:17 |
Overview of materials for Polystyrene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Flame Retardant". Each property range of values reported is minimum and maximum values of a.. |