Polymer Property : Deflection Temperature at 0.46 MPa (66 psi) = 139 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 59.5 °C
139 °F
ASTM D648
LyondellBasell Alathon® H4250 High Density Polyethylene, Injection Molding Grade
ALATHON H4250 is a high-flow “freezer” grade resin that exhibits enhanced cold temperature impact performance, enhanced processing and thermal stability, with good color and organoleptic p..